Spall Repair by the Preplaced Aggregate Method (RA ...
Spall Repair by the Preplaced Aggregate Method (RAP 9)
Create Account
Availability
On-Demand
Access expires 180 days after start
Cost
$0.00
Credit Offered
0.1 CEU Credit
1 PDH Credit
Course Description
This module is based on RAP9(05)(Reapproved 2010)- Spall Repair by the Preplaced Aggregate Method. The document is intended as a voluntary field guide for the owner, design professional, and concrete repair contractor interested in repairing concrete using preplaced aggregate concrete. The document was developed by ACI Committee E706 and approved by the ACI Educational Activities Committee.
Learning Objectives
1. List the benefits of preplaced aggregate concrete.
2. Describe the types of repairs that can benefit from this method.
3. Explain the pumping techniques and procedure.
4. Determine the proper surface moisture conditions of substrate concrete.
Instructions
Read and study the materials included in this module. Then, complete and pass the corresponding 10-question quiz with a score of 80% or higher to receive a certificate for 0.1 CEU (equivalent to 1.0 PDH).Continuing Education Credit: 0.1 CEU (1.0 PDH)Approved AIA and ICCAccess Period: 180 days
×